Measurement |
Condition |
Value |
Viscosity |
@ 25.5 °C (77.9 °F) |
546 cps |
Color |
Canary yellow |
|
Density |
@ 25 °C (77 °F) |
1.127 g/cm³ |
Ec(critical exposure) |
Dp(slop of cure-depth vs.ln(E) curve) |
9.33 mJ/cm2 |
0.13 |
ASTM Method |
Property Description |
Value |
ASTM D 638 |
Tensile Modulus |
1271.3 MPa |
ASTM D 638 |
Tensile Strength at Break |
59.75 MPa |
ASTM D 638 |
Elongation at Break |
4.7% |
ASTM D 648 @66PSI |
Heat Deflection Tempertature |
60 ℃ |
ASTM D 790 |
Flexural Strength |
44.71Mpa |
ASTM D 790 |
Flexural Modulus |
951.2Mpa |
ASTM D 256 |
Izod Impact (Notched) |
38.44 J/m |
ASTM D 2240 |
Hardness Shore D |
82 |
Subject | Download | View |
ProtoFab Magna L90 | ||
ProtoFab Magna L90 MSDS |